editDescriptionCasting ingot defects killed and rimmed steels.PNG |
English: Casting ingot defects. Comparison between killed steels and rimmed steels.
Français : Défauts de moulage dans un lingot. comparaison entre des aciers "calmés" et des aciers "effervescents". |
Source | The Manufacture Of Iron And Steel Vol II p.292 |
Author | Reginald Bashforth G. |
Permission (Reusing this file) |
see archive.org |
Licensing
editPublic domainPublic domainfalsefalse |
![]() |
This media file is in the public domain in the United States. This applies to U.S. works where the copyright has expired, often because its first publication occurred prior to January 1, 1929, and if not then due to lack of notice or renewal. See this page for further explanation.
|
![]() |
![]() |
This image might not be in the public domain outside of the United States; this especially applies in the countries and areas that do not apply the rule of the shorter term for US works, such as Canada, Mainland China (not Hong Kong or Macao), Germany, Mexico, and Switzerland. The creator and year of publication are essential information and must be provided. See Wikipedia:Public domain and Wikipedia:Copyrights for more details.
|
File history
Click on a date/time to view the file as it appeared at that time.
Date/Time | Thumbnail | Dimensions | User | Comment | |
---|---|---|---|---|---|
current | 21:29, 30 June 2012 | 1,177 × 641 (299 KB) | Borvan53 (talk | contribs) |
You cannot overwrite this file.
File usage on Commons
The following page uses this file: