DescriptionFinishtestHolz.png |
English: Test of various wood finishes: Varnishes, oils and waxes. The test pieces are maple wood and weigh 25 g on average. The edges are rounded to avoid weak spots in the finishes. After applying the finish the pieces were stored for four months. For testing I put them into water for several hours and continuously measured their weight to determine the water absorption. The test arose in the forum Fletcher’s Corner.
Deutsch: Test verschiedener Oberflächenbehandlungen von Holz mit Lacken, Ölen und Wachsen. Die Teststücke sind aus Ahornholz und durchschnittlich 25 Gramm schwer, mit abgerundeten Kanten, und wurden nach der Oberflächenbehandlung 4 Monate gelagert, ehe sie getestet wurden. Die Hölzer habe ich dann während mehreren Stunden ins Wasser gelegt und die Gewichtsveränderung (d. h. Wasseraufnahme) gemessen. Der Test entstand ursprünglich im Forum Fletcher’s Corner.
|
Date | |
Source | Own work |
Author | Simon A. Eugster |
Other versions |
|
Other licensing InfoField | If you wish to use this picture under a different license, e.g. for a book, please contact me. |
Licensing edit
I, the copyright holder of this work, hereby publish it under the following licenses:
Permission is granted to copy, distribute and/or modify this document under the terms of the GNU Free Documentation License, Version 1.2 or any later version published by the Free Software Foundation; with no Invariant Sections, no Front-Cover Texts, and no Back-Cover Texts. A copy of the license is included in the section entitled GNU Free Documentation License.http://www.gnu.org/copyleft/fdl.htmlGFDLGNU Free Documentation Licensetruetrue |
This file is licensed under the Creative Commons Attribution-Share Alike 3.0 Unported license.
- You are free:
- to share – to copy, distribute and transmit the work
- to remix – to adapt the work
- Under the following conditions:
- attribution – You must give appropriate credit, provide a link to the license, and indicate if changes were made. You may do so in any reasonable manner, but not in any way that suggests the licensor endorses you or your use.
- share alike – If you remix, transform, or build upon the material, you must distribute your contributions under the same or compatible license as the original.
You may select the license of your choice.
File history
Click on a date/time to view the file as it appeared at that time.
Date/Time | Thumbnail | Dimensions | User | Comment | |
---|---|---|---|---|---|
current | 08:17, 6 July 2012 | 1,277 × 2,000 (203 KB) | LivingShadow (talk | contribs) | Redone | |
15:34, 28 January 2012 | 3,004 × 1,644 (132 KB) | LivingShadow (talk | contribs) | {{Information |Description= {{de|Test verschiedener Oberflächenbehandlungen. Die Teststücke waren durchschnittlich 25 Gramm schwere Ahornhölzer mit abgerundeten Kanten und wurden nach der Oberflächenbehandlung 4 Monate gelagert, bis sie getestet wurde |
You cannot overwrite this file.
File usage on Commons
The following 15 pages use this file:
- User:LivingShadow/ TemplateWoodenFinishesGallery
- File:FinishtestHolz.png
- File:Piece01-LinseedOil.jpg
- File:Piece02-ShellacOrange.jpg
- File:Piece03-CarnaubaBeeWax.jpg
- File:Piece04-NoFinish.jpg
- File:Piece05-BeeWax-Molten.jpg
- File:Piece06-Shellac-LinseedOil.jpg
- File:Piece07-Acrylic-Paint.jpg
- File:Piece08-PUR-Alkyd-Varnish.jpg
- File:Piece09-Spar-Varnish.jpg
- File:Piece10-TungOil.jpg
- File:Piece11-TungOil-LinseedOil.jpg
- File:Piece12-PU-Acrylic-Varnish.jpg
- File:Varnish peeling off.jpg
File usage on other wikis
The following other wikis use this file:
- Usage on de.wikipedia.org
- Usage on de.wikibooks.org
Metadata
This file contains additional information such as Exif metadata which may have been added by the digital camera, scanner, or software program used to create or digitize it. If the file has been modified from its original state, some details such as the timestamp may not fully reflect those of the original file. The timestamp is only as accurate as the clock in the camera, and it may be completely wrong.
Horizontal resolution | 100.96 dpc |
---|---|
Vertical resolution | 100.96 dpc |
Software used |